W/O Sun Protection Soft Cream
Dostawca: EVONIK
Receptura:
| Phase | Ingredients | INCI Name | % w-w |
| A | ISOLAN® PDI | Diisostearoyl Polyglyceryl-3 Dimer Dilinoleate | 3.0 |
| A | ABIL® Wax 9840 | Cetyl Dimethicone | 0.25 |
| A | TEGOSOFT® TN | C12-15 Alkyl Benzoate | 7.0 |
| A | TEGO® Alkanol 1618 | Cetearyl Alcohol | 1.0 |
| A | Mineral Oil (30 mPas) | Mineral Oil (30 mPas) | 4.25 |
| A | Cyclomethicone | Cyclomethicone | 10.0 |
| A | Hydrogenated Castor Oil | Hydrogenated Castor Oil | 0.5 |
| A | Paracera W 80 | Microcrystalline Wax, Paramelt B.V. | 0.5 |
| A | Isostearic Acid | Isostearic Acid | 1.0 |
| A | Ethylhexyl Methoxycinnamate | Ethylhexyl Methoxycinnamate | 5.0 |
| A | Parsol SLX | Polysilicone-15, Roche-Vitamins | 3.0 |
|
A |
Tocopheryl Acetate | Tocopheryl Acetate | 0.5 |
| B | TEGO® Sun Z 800 | Zinc Oxide; Trimethoxycaprylylsilane | 5.0 |
| C | Glycerin | Glycerin | 2.0 |
| C | Phenylbenzimidazole Sulfonic Acid | Phenylbenzimidazole Sulfonic Acid | 3.0 |
| C | Sodium Chloride | Sodium Chloride | 0.50 |
| C | Sodium Hydroxide (10 % in water) | Sodium Hydroxide | 4.4 |
| C | Water | Water | 50.1 |
Procedura wykonania:
1. Heat phase A to approx. 80 °C.
2. Add phase B and disperse the pigment.
3. Add phase C (80 °C or room temperature) slowly while stirring.
4. Homogenise for a short time.
Cool with gentle stirring below 30 °C and homogenise again.